I'm talking about in the product diy and I am sure that no one on the forum has ever used, therefore, a need to try to credere.Lo made use you to my friends and now when the end will come to me to ask for it.
I'm talking about in the product diy and I am sure that no one on the forum has ever used, therefore, a need to try to credere.Lo made use you to my friends and now when the end will come to me to ask for it.
There capit? after you have done welding, you can not pi? cliffs the pond? Happens to me often, it becomes opaque, and I find it hard to do so riscogliere.
it seems that to become iron! but how ? can?
I use the flux stagnosald, then I have a nice stock pond, the old-style lead-acid (40/60) which, unfortunately, I do not sell more? because of the new products Lead-Free!!! The problem of the paste type my ? if putacaso the heat in the wrong place this Friday at the risk of making something out of it!!!
hi guys,for curiosity? where the pond used to speak of the quality? good, if possible to have some links, even in the pm!! thanks
You do not really understand something until you can explain it to your grandmother (Einstein)
keep 60/40 let go of the pond eco-friendly serves no purpose...
the mixture of ammonium Chloride (NH4Cl) and glycerin-this is the medicine for your problema.leggi the 1 post.
in the specialized shops for mural painting, you should find it!
To clean I use pure Acetone, it evaporates immediately, and to a good result. Use 2 Flux, a liquid and a cream. For the pond I made a stash of 40/60 and why? the new one they sell, doesn't it ? the maximum of the welds on the fly. I have 6 welders, of which the JBC that ? the top, it costs 500 euros, but the welds are guaranteed. Among the welders in the pi? of elite I have a station BGA IR, but the use for the repair of the PC, and use the flux to the cream of the AMTEC, and then I clean everything with acetone and "cotonfioc"